FIOLAX® clear

 - Tubing for ampoules

FIOLAX® clear
 
FKO AW12.75±0.12/0.50±0.02 1500 010 200
1029017
Product Details
12.750 +/- 0.120

11.750

0.500 +/- 0.020

1,500.000

67.5

17.0

54

918.0

252

6

 