Slimline features and surface appeal
SCHOTT MEMpax® extends the world’s renowned BOROFLOAT® borosilicate glass thickness portfolio in extremely low thicknesses, from 0.07-0.55 mm. It also benefits from a pristine, fire-polished surface, removing the need for grinding and polishing, and can be used anywhere that extremely thin borosilicate glasses are required, such as MEMS and biotechnology applications.
![SCHOTT MEMpax® is ideal for lab-on-a-chip systems in diagnostics and life science applications Hand holding an ultra-thin glass sheet with lab-on-a-chip system](/-/media/project/onex/products/m/mempax/product-highlights/m-72968_690x470.jpg?rev=b1dd176d0e3a4ff6bd2041919528e148)
Outstandingly versatile
A combination of unique thicknesses and outstanding properties expand the potential of MEMpax®. Its CTE (coefficient of thermal expansion) corresponds to a silicon wafer, which makes it ideal for wafer applications in anodic and other bonding processes. Low autofluorescence, high UV transmission, and electrically non-conductive properties further widen its potential.
Unique portfolio of properties
MEMpax® enables a range of shapes and sizes to be combined with unrivalled low thicknesses, while very high chemical resistance makes this high purity glass extremely durable during processing. Its CTE makes it highly compatible with silicon in bonding processes, its high (UV) transmission allows fast debonding, and it maintains non-electrical conductivity even at high temperatures.
We are certified
We are both ISO 9001 and 14001 certified. The production of MEMpax® is constantly monitored at all stages and all our glass is subjected to stringent quality inspection before shipping. It also complies with EU-RoHS and EU-REACH standards.