Product Variants of DURAN®
DURAN® Tough
For partition walls and modern lighting, there’s a demand for glass that combines strong safety features with high visual clarity. DURAN® Tough was developed for interior and exterior design, offering all the elegance, strength, and geometric precision of DURAN® glass tubing with an additional polymer coating for improved safety.
CHARACTERISTICS
Applied to the inner surface of the glass tube, the clear polymer coating ensures that the DURAN® Tough tubing maintains its form and integrity in the event of breakage, providing crucial protection against glass splinters and shards. Since DURAN® glass absorbs UV radiation, the coating is protected from UV degradation and remains stable in a wide range of environments.
YOUR ADVANTAGES
- High transparency and visual quality for architectural and industrial design.
- Precise geometric tolerances for accurate fitting.
- Product integrity retained if broken, considerably reducing the risk of injury.
- Available with an outside diameter of 120 mm in lengths from 1,500 to 4,000 mm.
DURAN® in Jumbo Size
The world-famous DURAN® borosilicate glass tubing can be processed with an outer diameter of up to 465 mm – a world record! This jumbo-sized DURAN® retains the high quality and technical properties of smaller DURAN® tubing, so is ideal for large-scale glass apparatus constructions such as chemical reactors.
CHARACTERISTICS
Since jumbo-sized DURAN® glass tubing is manufactured using the same direct-draw process as standard DURAN® tubing, it offers the same strength, tight tolerances, chemical and electrical resistance, optical quality, and thermal shock resistance.
YOUR ADVANTAGES
- High quality glass tubing with large outer diameter.
- Tight tolerances and high mechanical strength.
DURATAN®
On average, this thermally prestressed variant of DURAN® offers a higher level of mechanical resistance than the regular DURAN® range. With impact and stress resistance more than doubled (on average), DURATAN® is ideal for highly challenging applications.
High scratch resistance and strong light transmission properties also make this variant ideal for external use, and a fine break pattern improves the safety characteristics of the glass as it breaks in a less hazardous way.
YOUR ADVANTAGES
On average 2-3 times higher resistance to tensile stress and mechanical impact compared to DURAN®.
Fine break pattern, similar to tempered safety glass (ESG).