Technical Details for Proteon™ by SCHOTT Primoceler Oy
Specifications
Hermeticity and biocompatibility of Proteon™ packages for implants are based on three key factors:- laser-based Primoceler® Glass Micro Bonding
- HermeS® hermetic through-glass-vias for electrical feedthroughs, and
- Borofloat® 33 biocompatible glass.
Parameter | Specification |
---|---|
Glass type |
|
Glass thickness |
|
Hermeticity level for glass micro bonding |
|
Hermeticity level for HermeS® |
|
Glass micro bonding sealing temperature |
|
Gas backfill and pressure |
|
Implant package size |
|
Implant package shape |
|
Metallization |
|
Through-glass-via material |
|
Electronics assembly on glass |
|
Gap between glass layers / additional materials |
|
Optical / dielectric coatings |
|
Parameter | Specification |
---|---|
Glass type |
|
Glass thickness |
|
Hermeticity level for glass micro bonding |
|
Hermeticity level for HermeS® |
|
Glass micro bonding sealing temperature |
|
Gas backfill and pressure |
|
Implant package size |
|
Implant package shape |
|
Metallization |
|
Through-glass-via material |
|
Electronics assembly on glass |
|
Gap between glass layers / additional materials |
|
Optical / dielectric coatings |
|