Glasses are assigned to glass families according to their position in the Abbe diagram. Environmentally friendly glasses are marked with the suffix "N-" or "P-" against the classic glasses. Prefixes such as "HT" or "HTultra" denote glasses with a high minimum transmission in the UV-near spectral range.
|
L
Length in mm
|
W
Width in mm
|
T
Thickness in mm
|
DIA
Diameter in mm
|
Step
nd |
Step
vd |
nd
Refractive index at the yellow helium line at 587.5618 nm
|
vd
Abbe number is a measure for the dispersion. It is calculated by νd=(nd-1)/(nF-nC)
|
Weight
Weight (KG) greater than half is rounded up without taking tolerances into consideration.
|
|
---|
The checkbox can only be used for a product request. To order the article please press the "Select" button.
|
SCHOTT
Article |
Glass type
Glasses are assigned to glass families according to their position in the Abbe diagram. Environmentally friendly glasses are marked with the suffix "N-" or "P-" against the classic glasses. Prefixes such as "HT" or "HTultra" denote glasses with a high minimum transmission in the UV-near spectral range.
|
L
Length in mm
|
W
Width in mm
|
T
Thickness in mm
|
DIA
Diameter in mm
|
Step
nd |
Step
vd |
nd
Refractive index at the yellow helium line at 587.5618 nm
|
vd
Abbe number is a measure for the dispersion. It is calculated by νd=(nd-1)/(nF-nC)
|
Weight
Weight (KG) greater than half is rounded up without taking tolerances into consideration.
| |
---|---|---|---|---|---|---|---|---|---|---|---|---|
|
1136676
| N-KZFS8 |
280
+20 -0 |
160
+5 -0 |
40
+10 -0 |
| 1 | 1 | 1.72047 | 34.70 | 6 |
Select
<div class="anonymous-user-overlay flex-grow-1">
<div class="h6 mb-4">
Sign in to choose your product</div>
<p>As a registered user in our shop you enjoy many advantages</p>
<ul>
<li>Simply order</li>
<li>Stock overview</li>
<li>Simple profile management</li>
</ul>
<div class="d-md-flex 11justify-content-between">
<form id="command" class="mr-md-3" action="/shop/advanced-optics/en/schottid/login" method="get"><button class="btn btn-primary anonymous-overlay-button js-login-submit-button mt-3 w-100"
data-ga-track-custom-login='{"event":"login","login_method":"standard","login_status":"logged out"}'>
Login</button>
</form><form id="command" action="/shop/advanced-optics/en/schottid/register" method="get"><button class="btn btn-secondary anonymous-overlay-button mt-3 js-ga-tracking w-100"
data-ga-track-click='{"event":"click","element_type":"button","element_name":"Create account","link_url":"/shop/advanced-optics/en/schottid/register"}'>
Create SCHOTT ID</button>
</form></div>
</div>
|
|
1476221
| N-KZFS8 |
280
+20 -0 |
160
+5 -0 |
40
+10 -0 |
| 0.5 | 0.5 | 1.72047 | 34.70 | 6 |
Select
<div class="anonymous-user-overlay flex-grow-1">
<div class="h6 mb-4">
Sign in to choose your product</div>
<p>As a registered user in our shop you enjoy many advantages</p>
<ul>
<li>Simply order</li>
<li>Stock overview</li>
<li>Simple profile management</li>
</ul>
<div class="d-md-flex 11justify-content-between">
<form id="command" class="mr-md-3" action="/shop/advanced-optics/en/schottid/login" method="get"><button class="btn btn-primary anonymous-overlay-button js-login-submit-button mt-3 w-100"
data-ga-track-custom-login='{"event":"login","login_method":"standard","login_status":"logged out"}'>
Login</button>
</form><form id="command" action="/shop/advanced-optics/en/schottid/register" method="get"><button class="btn btn-secondary anonymous-overlay-button mt-3 js-ga-tracking w-100"
data-ga-track-click='{"event":"click","element_type":"button","element_name":"Create account","link_url":"/shop/advanced-optics/en/schottid/register"}'>
Create SCHOTT ID</button>
</form></div>
</div>
|
|
1290908
| N-KZFS8 |
280
+20 -0 |
160
+5 -0 |
40
+10 -0 |
| 3 | 3 | 1.72047 | 34.70 | 6 |
Select
<div class="anonymous-user-overlay flex-grow-1">
<div class="h6 mb-4">
Sign in to choose your product</div>
<p>As a registered user in our shop you enjoy many advantages</p>
<ul>
<li>Simply order</li>
<li>Stock overview</li>
<li>Simple profile management</li>
</ul>
<div class="d-md-flex 11justify-content-between">
<form id="command" class="mr-md-3" action="/shop/advanced-optics/en/schottid/login" method="get"><button class="btn btn-primary anonymous-overlay-button js-login-submit-button mt-3 w-100"
data-ga-track-custom-login='{"event":"login","login_method":"standard","login_status":"logged out"}'>
Login</button>
</form><form id="command" action="/shop/advanced-optics/en/schottid/register" method="get"><button class="btn btn-secondary anonymous-overlay-button mt-3 js-ga-tracking w-100"
data-ga-track-click='{"event":"click","element_type":"button","element_name":"Create account","link_url":"/shop/advanced-optics/en/schottid/register"}'>
Create SCHOTT ID</button>
</form></div>
</div>
|
Showing results 1 - 3 of 3